By diret measuremnts we demonstrated that in inorganic PLZT thin films and organic polymer ferroelectric the electrocaloric effect can exceed 40 K.
COBISS.SI-ID: 24060199
We show that indirect measurements do not give proper results of electrocaloric response in relaxor feroelectric polymers.
COBISS.SI-ID: 24168999
We show that the electrocaloric effect exhibits a maximum at the ferroelectric-paraelectric transition in ferroelectric poly(vinylidene-fluoride/trifluoroethylene) 55/45 mol % copolymer.
COBISS.SI-ID: 24585255
We solve the decades old problem about the ground state of relaxor ferroelectrics by showing that it is the glassy state and not random-field frozen ferroelectric state.
COBISS.SI-ID: 25971495
We calculated theoretically the upper bond on the electrocaloric effect in polar solids
COBISS.SI-ID: 24382759